กก
Magnesia
Raw Material |
 |
 |
 |
 |
Magnesia Raw Material
Its refractory materials made with artificial
synthesis techniques have the advantages of quality consistency
and adjustable elements, they have long service life and save
energy, are functional and pollution free. |
|
|
|
|
SYNTHETIC MAGNESIAL
DOLOMITE CLINKER |
 |
 |
|
 |
|
Brand |
MgO,% |
CaO,% |
SiO2+Fe2O3+Al2O3,% |
Loss on ignition |
Bulk density |
|
MBS-74A |
≥74 |
≥20 |
≤3.0 |
≤0.8 |
≥3.30 |
|
MBS-74B |
≥74 |
≥20 |
≤3.0 |
≤0.8 |
≥3.30 |
|
 |
 |
|
|
MAGNESIAL ALUMINA
SPINEL |
 |
 |
|
 |
|
MgO,% |
Al2O3,% |
SiO2,% |
Fe2O3,% |
CaO,% |
Loss on ignition |
Bulk density |
|
27-30 |
60-65 |
≥4.5 |
≤1.8 |
≤1.0 |
≤0.5 |
≥3.10 |
|
 |
 |
|
|
SYNTHETIC
MAGNESIAL CALCIA
FERRIC OXIDE CLINKER |
 |
 |
|
 |
|
Brand |
MgO,% |
Fe2O3,% |
CaO,% |
SiO2,% |
Al2O3,% |
Loss on ignition |
Bulk density |
|
MGFS-80 |
80-82 |
5-7 |
10-12 |
≤1.1 |
≤0.5 |
≤1.0 |
≥3.30 |
|
MGFS-78 |
78-80 |
5-7 |
10-12 |
≤2.0 |
≤0.7 |
≤1.0 |
≥3.25 |
|
|
|
|
 |
SYNTHETIC
MAGNESIAL THREE
CALCIA CLINKER |
|
|
 |
|
MgO,% |
CaO,% |
SiO2+Fe2O3+Al2O3,% |
CaO/SiO2 |
Loss on ignition |
Bulk density |
|
≥90 |
≤6 |
≤3.6 |
≥3 |
≤0.4 |
≥3.25 |
|
|
|
|
 |
MAGNESITE
CLINKER |
|
|
 |
|
Brand |
MgO,% |
CaO,% |
SiO2,% |
Loss on ignition |
Bulk density |
|
MS-95 |
≥95 |
≤1.5 |
≤2.0 |
≤0.5 |
≥3.15 |
|
MS-90 |
≥90 |
≤2.0 |
≤5.0 |
≤0.3 |
≥3.20 |
|
MS-87 |
≥87 |
≤2.0 |
≤7.0 |
≤0.5 |
≥3.20 |
|
MS-84 |
≥84 |
≤2.0 |
≤9.0 |
≤0.5 |
≥3.20 |
|
|
|
|
 |
LIGHT BURNED
MAGNESIA |
|
|
 |
|
Brand |
QM-94 |
QM-92 |
QM-85 |
QM-80 |
QM-75 |
|
MgO,% |
≥94 |
≥92 |
≥85 |
≥80 |
≥75 |
|
SiO2,% |
≤1.2 |
≤3.0 |
≤6.0 |
≤8.0 |
≤10 |
|
Loss on ignition |
≤3.0 |
≤3.0 |
≤6.0 |
≤10 |
≤12 |
|
Grain size,mm |
≤0.125 |
≤0.125 |
≤0.125 |
≤0.125 |
≤0.125 |
|
|
|
|
 |
MAGNESITE |
|
|
 |
|
Grade |
MgO,% |
SiO2,% |
CaO,% |
Fe2O3,% |
Lumpiness |
|
First grade |
≥46 |
≤2.5 |
≤0.8 |
≤0.7 |
50-350 |
|
Second grade |
≥45 |
≤4.5 |
≤1.0 |
≤1.0 |
50-350 |
|
Third grade |
≥44 |
≤6.0 |
≤2.0 |
≤1.0 |
50-350 |
|
|
|